P.540
| FIBER PROTECTOR TEST RESULTS | 
| 1.TENSILE STRENGTH TEST | 2.COMPRESSION BREAKING LOAD TEST | 3.BEND-BREAKING LOAD TEST | 4.TEST CERTIFICATE | 
2.COMPRESSION BREAKING LOAD TEST
| METHOD OF TEST | PURPOSE OF THE TEST | 
| COMRESS 100mm FIBER PROTECTOR 1mm/MINUTE UNTIL IT BEGINS DEFORMED. THE RESULT ON THE TABEL IS COMPRESSION BREAKING LOAD WEIGHT.  | 
      TO GET DATA OF COMPRESSION BREAKING LOAD WEIGHT THAT FIBER PROTECTOR BEGIN TO DEFORMED. | 
![]()  | 
      ![]()  | 
    
| RESULTS | These tests were performed by IS-10T and RS-2 made by Shimazu Co., Ltd
      at Chibaken Mechanical-Metal Examination Institute and Tokyo-Metropolitan-Mechanical-Technology
      Center on 08/28/1989. Observer: Shimizu, Hagitec Co., Ltd. *Remarks*@These datas are only for reference for the products.  | 
    
    ||
| TYPE | Range/kg | Load/kg | |
| KS-1.8N | 2000 | 600 | |
| KS-5N | 2000 | 540 | |
| KS-7N | 2000 | 340 | |
| SA-4N | 2000 | 830 | |
| IS-4N | 2000 | 1100 | |
| SX-8N | 2000 | 1150 | |
| SASP-8.5N | 2000 | 760 | |